Chrome Cobalt Alloy

Evacryl Economy Rod CE (BB03)

Evacryl CoCr Economy

 

 

 

Co 62.5%

Cr 28.5%
Mo 6.0%

Casting Temperature 1482°C
Proof Stress 699 MPa
Elongation 6%

 Beta Plus CE (BB04)

Very high quality chrome cobalt alloy, pure enough for implant work.

Co 61%
Cr  31%
Mo 6%
Casting temp 1482°C
Proof stress   591
Elongation      3%

Advance Chrome CE (BB05)

Premium chrome cobalt alloy
Co 64%
Cr  28.5%
Mo 5%
Casting temp  1510°C
Proof stress    64500%
Elongation       13%